Post breakage balustrade load test

Max. collapse load test on broken laminated glass balustrade at Eminent Test Lab in Hyderabad, India.

After the line load test, both glass layers of each specimen & sample type were broken using a centre punch. Post the breakage, point load was applied at the middle of the top edge to record the maximum load required to cause complete collapse. Trosifol® Extra Stiff Pro required a larger bending force to cause complete collapse compared to the competitive product.