After the line load test, both glass layers of each specimen & sample type were broken using a centre punch. Post the breakage, point load was applied at the middle of the top edge to record the maximum load required to cause complete collapse. Trosifol® Extra Stiff Pro required a larger bending force to cause complete collapse compared to the competitive product.